Dense multilayer high-speed switch board with three BGA cavities, built on Megtron ultra-low-loss laminate

High Speed PCB Manufacturing

High-Speed PCB Manufacturer Signal Integrity to 112G PAM4

PCB fabrication engineered for 56G and 112G SerDes channels. Ultra-low-loss materials, precision impedance control, optimized via structures, and verified insertion loss on every production lot.

112G
PAM4 / Lane
40
Max Layers
±0.1mm
Back-Drill Accuracy
±5%
Impedance Tol.

Capabilities

High Speed PCB Capabilities

Everything your 56G/112G channel needs from the board.

Df down to 0.0005

Ultra-Low-Loss Materials

Full Megtron ladder (6 / 7 / 8 / 9) plus Astra MT77, IT-968SE, S7439. Hybrid stackups with FR-4 on non-critical layers to reduce cost.

±0.1mm accuracy

Back-Drilling

CNC-controlled stub removal on through-hole vias. Depth accuracy ±0.1mm. Cross-section verified on first article.

±8% / ±5%

Impedance Control

Single-ended and differential ±8% tolerance standard. Enhanced ±5% available. TDR tested 100%.

HVLP / HVLP2

Low-Roughness Copper

HVLP and HVLP2 foils (Rz under 2-3um) for inner and outer layers. Reduces conductor loss 15-25% vs standard ED copper.

Up to 40L

High Layer Count

Up to 40 layers with sequential lamination. Tight registration for pad-on-via alignment across 20+ layer transitions.

Optional S21 report

Insertion Loss Testing

VNA-based insertion loss measurement on test coupons. Verifies that production boards meet your loss budget per inch.

Per your spec

Anti-Pad Optimization

Non-functional pad removal (NPTH) and optimized anti-pad geometry to minimize via-to-trace coupling and return loss.

Spread glass available

Glass Weave Mitigation

Spread-glass prepreg and trace rotation options to reduce fiber-weave skew on differential pairs above 25 Gbps.

Hybrid stackups

Mixed Dielectric Stackup

Combine ultra-low-loss laminates on signal layers with standard FR-4 on power/ground. Saves 30-50% vs all-low-loss.

Signal Integrity

Why High Speed PCB Is Different

At 28 Gbps NRZ and above, the PCB is no longer just a mechanical carrier for components. It becomes the dominant contributor to channel loss. A standard FR-4 board running at 56 Gbps PAM4 will lose 1.0-1.5 dB/inch on inner-layer striplines, which exhausts most transceiver equalization budgets before the signal reaches the receiver. High speed PCB manufacturing treats the board as a transmission line system from the first day of stackup planning through final electrical verification.

The challenge is threefold. First, dielectric loss in the substrate material dominates above 10 GHz, so the laminate selection determines whether your channel will close. Second, copper roughness on the trace surface adds 0.2-0.5 dB/inch at 28 GHz depending on foil type, and this roughness is invisible in your EDA tool. Third, via stubs, even 5-mil stubs left by incomplete back-drilling, create resonances that destroy signal integrity at specific frequencies. Managing all three variables simultaneously, in production at volume, is what separates a high speed PCB manufacturer from a standard one.

Dielectric Loss Control

We build the full Panasonic Megtron ladder — Megtron 6 (Df 0.004), Megtron 7 (Df 0.002), Megtron 8 (Df 0.0008), and Megtron 9 (Df 0.0005) — alongside Isola Astra MT77 (Df 0.0017), ITEQ IT-968SE (Df 0.0015), and Shengyi S7439 (Df 0.0013). Material selection is matched to your data rate and channel length. At 112G PAM4, one step on that ladder is the difference between a channel that closes and one that fails.

Copper Roughness Management

Standard electrodeposited copper (ED foil) has Rz roughness of 5-8um. At 28 GHz, that adds 0.3-0.5 dB/inch to your loss budget. We offer HVLP (Rz under 3um) and HVLP2 (Rz under 2um) foils as standard options for high speed stackups. The roughness is specified on your stackup drawing and verified by cross-section.

Via Stub Elimination

Via stubs above 10 mil create quarter-wave resonances below 20 GHz that appear as deep notches in your S21 plot. We back-drill every high speed via to within 0.1mm of the target layer, verified by cross-section on first article. For designs above 56G, we recommend blind/buried via structures that eliminate stubs entirely.

Insertion Loss Verification

VNA-based insertion loss measurement on test coupons matched to your actual trace geometry verifies that production boards meet your loss budget per inch — catching material lot-to-lot variation before it reaches your assembly line.

Multi-up high-speed production panel with dense BGA arrays and controlled-impedance routing on ultra-low-loss laminate

High-Speed Boards We Build

Controlled-impedance multilayers, in the wild

Three high-speed modules with gold-plated pads, edge contacts, and dense BGA fields
Gold-plated module array
Dense multilayer switch board with three large BGA cavities on ultra-low-loss laminate
Switch board, three BGA cavities
Multi-up high-speed production panel carrying two board designs, four boards total
Multi-up production panel
Macro of gold-finger edge connector contacts and impedance-controlled traces
Gold-finger edge connector
Blue trays of finished high-speed PCB modules packed for shipment
Production volume, packed
Fine-pitch HDI PCB with dense BGA fan-out for high-speed signaling
HDI BGA fan-out

Manufacturing Process

From Stackup Review to Verified Loss

Every high speed PCB order begins with a stackup review and ends with electrical verification. Here is what happens on our floor — and why each control matters for your loss budget.

01

Stackup & Channel Review

Every order begins with a stackup review — we model your target impedance and estimate insertion loss per inch from your chosen material and copper roughness, confirming fabrication can deliver what your channel simulation predicts.

02

Material Selection

The laminate is matched to your data rate and channel length — Megtron 6 for 56G, Megtron 7 for 112G, Megtron 8/9 for 224G and CPO, or the Astra MT77 / IT-968SE / S7439 equivalents. One grade on the Megtron ladder decides whether the channel closes.

03

Impedance-Controlled Fabrication

Single-ended and differential lines built to ±8% standard (±5% enhanced) and TDR tested 100%. Etch factor and dielectric height are held tight so measured impedance matches the stackup model.

04

Sequential Lamination

Up to 40 layers with sequential lamination, holding registration tight enough for pad-on-via alignment across 20+ layer transitions on low-loss laminate.

05

Back-Drilling with X-ray Depth Control

Back-drill depth is set by X-ray measurement of inner-layer position on each panel — not a fixed depth from the board surface — compensating for lamination thickness variation and holding stub length below 5 mil at ±0.1mm.

06

Pre-Production Test Vehicle

For 112G PAM4 designs we run pre-production test vehicles to verify insertion loss before committing your full lot, catching material lot-to-lot variation, etch factor drift, and plating thickness effects before assembly.

07

Insertion Loss Verification

VNA-based S-parameter measurement on coupons matched to your trace geometry reports insertion loss (S21) and return loss (S11) from DC to your Nyquist frequency, per-lot or per-panel.

08

Finish & Final Electrical Test

Solder mask, surface finish, and full electrical test complete the board, with first-article cross-sections confirming back-drill depth and impedance on every new design.

Dense multilayer high-speed switch board on Megtron 7 laminate, with three large BGA cavities and back-drilled high-speed vias

Materials & Stackup

Matched to your data rate and channel length

Choosing the right laminate is the single decision that determines whether your channel closes. We build across the whole Panasonic Megtron ladder — Megtron 6 for 56G, Megtron 7 for 112G, Megtron 8 for 224G, and Megtron 9 for co-packaged optics — plus Isola, ITEQ, and Shengyi equivalents where availability or cost favours them, and standard FR-4 for short-reach DDR4 and USB 2.0.

Hybrid stackups place ultra-low-loss material only on the signal layers while keeping standard FR-4 on power and ground, cutting 30-50% off an all-low-loss construction with negligible impact on channel performance. The same trick works inside the Megtron family: Megtron 8 on the two or four 224G pairs, Megtron 6 everywhere else.

Megtron 6 Megtron 7 Megtron 8 Megtron 9 Astra MT77 IT-968SE S7439 HVLP2 copper
MaterialDkDfMax Data RateBest For
Megtron 92.90.0005224G+ PAM4Co-packaged optics, 448G prototyping
Megtron 8 (R-5785N)3.00.0008224G PAM451.2T+ switch fabric, AI/HPC backplanes
Megtron 7 (R-5785)3.30.002112G PAM4800G switches, AI accelerators
Megtron 6 (R-5775)3.40.00456G PAM4PCIe Gen5, 400GbE
ITEQ IT-968SE3.160.0015112G PAM4AI servers, HPC
Isola Astra MT773.000.0017112G PAM4Data center, 800GbE
Shengyi S74393.00.0013112G PAM4Cost-optimized 112G
Shengyi S7040G3.720.008928G NRZPCIe Gen4, 25GbE
Isola 370HR4.040.02110G NRZDDR4, USB 3.2, GbE
Standard FR-44.2-4.70.025-10GDDR4 short reach, USB 2.0

Not sure which material your channel budget requires? Send us your data rate, channel length, and equalization capability. Our SI engineers will model the channel and recommend the most cost-effective laminate. See our full material library for detailed datasheets.

Panasonic Megtron

Megtron 6, 7, 8 and 9 — which grade your channel actually needs

Megtron is the reference family for high-speed digital PCBs, and most of the boards on this page are built on it. The grades are not interchangeable: each step down the Df ladder roughly halves dielectric loss, and each step up the ladder costs more and takes longer to source. Choosing one grade too low means a channel that fails at temperature; one grade too high means paying two to three times the laminate cost for margin you will never use.

The rule of thumb we use in stackup review: multiply your per-inch insertion loss by the longest channel on the board, add 2 dB for connectors and vias, and compare against the transceiver's stated budget. If you are within 3 dB, move up a grade — production variation in resin content, etch factor, and copper roughness will eat that margin.

All four grades run on the same line here, with HVLP2 foil, back-drilling, and spread-glass prepreg available on each. Megtron 8 and 9 are allocation materials, so send your stackup early — we confirm mill availability before we confirm a date.

Three high-speed modules built on Panasonic Megtron laminate, with gold-plated pads and edge contacts

Design Guidelines

DFM for High-Speed Success

A handful of design choices decide whether your channel closes in production. These are the DFM recommendations our SI engineers apply to every high speed review.

Via Design

For signals above 25 Gbps, avoid through-hole vias routed on inner layers unless back-drilling is specified. Preferred: blind/buried vias or through-hole with back-drill. Anti-pad diameter should be 20 mil larger than drill diameter minimum to control return loss. Remove non-functional pads on all non-connected layers.

Trace Geometry

Target 4-5 mil trace width for 100-ohm differential stripline on Megtron 6 (Dk 3.4, 4 mil dielectric). Below 3.5 mil, etch factor variability starts to dominate impedance tolerance. Where possible, widen traces and increase dielectric height rather than shrink geometry. This reduces both loss and manufacturing risk.

Reference Plane Integrity

Every high speed trace must have an uninterrupted reference plane directly above or below. If the signal transitions layers (via), the return current must also transition via a nearby ground via within 20 mil. Split planes under differential pairs will cause common-mode conversion and EMI.

Material Specification

Specify the laminate system by name and grade, not by generic Dk/Df values. "Dk 3.4, Df 0.004" matches five different products with different mechanical and thermal properties. Call out the exact material and part number ("Panasonic Megtron 6 R-5775", "Megtron 8 R-5785N") and the foil type (HVLP or HVLP2) explicitly in your fab notes. On mixed-dielectric builds, name the material per layer pair — otherwise the stackup gets built to the cheapest reading of your note.

Macro view of gold-plated pads, fine-pitch component footprints, and a dense BGA field on high-speed modules

Applications

High-Speed Systems We Build For

We fabricate boards for these high speed systems daily.

AI / HPC Servers — high-speed PCB application

AI / HPC Servers

GPU interconnect backplanes at 112G PAM4, NVLink and PCIe Gen5/6 switch boards, AI training cluster fabric. Typically 20-32 layers on Megtron 7 (or Megtron 8 for 224G links) with HVLP2 copper.

Data Center Networking — high-speed PCB application

Data Center Networking

400G and 800G Ethernet switch line cards. Retimer boards, optical module host boards, and orthogonal midplane connectors. Channel loss budgets of 25-30 dB at Nyquist frequency. 51.2T+ fabrics move to Megtron 8.

5G Infrastructure — high-speed PCB application

5G Infrastructure

Baseband processing cards with 25G CPRI/eCPRI links. Fronthaul and midhaul interface boards. Mixed-material stackups combining Megtron 6 signal layers with standard power distribution.

High-Speed Test Equipment — high-speed PCB application

High-Speed Test Equipment

Oscilloscope front-end boards, BERT interposer cards, and channel emulation boards requiring insertion loss repeatability across production lots to within 0.1 dB/inch.

Automotive Ethernet — high-speed PCB application

Automotive Ethernet

In-vehicle 10GBASE-T1 and 25GBASE-T1 domain controllers. Zonal architecture backbone boards requiring low-loss with automotive-grade laminate (Tg 170+, CAF resistant).

Memory Modules — high-speed PCB application

Memory Modules

DDR5 RDIMM and LRDIMM substrates, CXL memory expander boards, and HBM interposers. Tight impedance matching (±5%) and length matching within 2 mil for data bus groups.

The Difference

Why High-Speed at AtlasPCB

The hard part of high speed isn't whether the board can be made — it's whether the finished channel matches your simulation. Our process is built around proving it does.

SI Engineering Review

Our SI engineers model your channel, estimate per-inch loss, and recommend material or geometry changes before you commit — free for production orders.

Verified Loss Budget

VNA insertion-loss testing on coupons matched to your trace geometry confirms production boards meet the loss budget your simulation predicted.

Back-Drill Precision

X-ray inner-layer measurement per panel holds stub length below 5 mil at ±0.1mm, killing the resonances that notch your S21 plot.

Full Megtron Ladder

Megtron 6, 7, 8, and 9 all run on our line — plus Astra MT77, IT-968SE, and S7439 — with hybrid stackups to place the expensive grade only where the channel needs it.

FAQ

High Speed PCB Questions

112 Gbps PAM4 per lane (800G Ethernet, PCIe Gen6) is routine volume work for us on Megtron 7 class laminate. 224 Gbps PAM4 is supported on Megtron 8 and Megtron 9 for qualified designs, subject to material allocation. The constraint at either rate is material selection and via structure, not our process capability — we will help you pick the combination that matches your target.

Megtron 6 (Df 0.004 at 10GHz) handles 28G NRZ and 56G PAM4 channels up to about 6-8 inches. For 112G PAM4, or 56G channels longer than 8 inches, move to Megtron 7 (Df 0.002 at 28GHz) or the Astra MT77 / IT-968SE equivalents. We can model your specific channel to confirm before you commit to a laminate.

Megtron 6 (Df 0.004) for PCIe Gen4/Gen5, 100GbE, and 56G under 8 inches. Megtron 7 (Df 0.002) for 112G PAM4 and 800G switching. Megtron 8 / R-5785N (Df 0.0008) for 224G PAM4 and 51.2T+ switch fabrics out to 12 inches. Megtron 9 (Df 0.0005, Dk 2.9) for co-packaged optics host boards and 448G prototyping. Each step down the ladder roughly halves dielectric loss and raises laminate cost, so we size the grade to your measured loss budget rather than defaulting to the top.

Megtron 8 and Megtron 9 are allocation materials from Panasonic, not shelf stock. We confirm mill availability before we confirm your delivery date; typical material lead time is 2-4 weeks. Megtron 6 and Megtron 7 are held in regular stock, though Megtron 7 depends on AGC T-Glass supply.

Yes, and for 224G designs it is usually the right answer. Megtron 8 goes on the two or four layer pairs carrying the fastest lanes, Megtron 6 or high-Tg FR-4 handles power, ground, and slow-speed routing. The grades share a compatible lamination cycle, so the mixed build does not add process risk — it just needs the stackup drawing to call out material per layer explicitly.

Ultra-low-loss materials (Megtron 6/7 class) typically add 40-80% to board cost versus standard FR-4, depending on layer count and panel size. Megtron 8 and 9 run higher again. Hybrid stackups (low-loss on signal layers, FR-4 on power/ground) reduce the premium to 25-45%, and the same approach works inside the Megtron family.

Yes. We offer VNA-based S-parameter measurement on test coupons matched to your actual trace geometry. The report gives you measured insertion loss (S21) and return loss (S11) from DC to your Nyquist frequency. Available per-lot or per-panel.

Our back-drilling uses X-ray measurement of actual inner layer position on each panel, then drills to within ±0.1mm (4 mil) of the target depth. Stub length is typically held below 5 mil. First article cross-sections confirm depth on every new design.

Yes, and we recommend them. Placing ultra-low-loss material only on signal layers while using standard FR-4 on power and ground layers saves 30-50% versus an all-low-loss construction, with negligible impact on channel performance.

Need high-speed PCBs?

Upload your Gerbers for an instant quote, or send your stackup for a free channel review before production.